System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Dow DMDB-7950 NT 7 High Density Polyethylene Resin
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
Material Notes:
DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short molding cycles.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.948
g/cc
0.0342
lb/in³
ASTM D792
ESCR 100% Igepal®
40
hour
@Temperature 50.0 °C
40
hour
@Temperature 122 °F
F
50
; Molded and tested in accordance with ASTM D4976; ASTM D1693
Melt Index of Compound
5.75
g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.75
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
54
54
Molded and tested in accordance with ASTM D4976; ASTM D2240
Tensile Strength at Break
26.2
MPa
3800
psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Tensile Strength, Yield
24.8
MPa
3600
psi
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Break
1200 %
1200 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Elongation at Yield
8.0 %
8.0 %
Molded and tested in accordance with ASTM D4976; ASTM D638
Flexural Modulus
1.01
GPa
@Strain 2 %
146
ksi
@Strain 2 %
Secant; Molded and tested per ASTM D4976; ASTM D790 B
Tensile Impact Strength
105
kJ/m²
50.0
ft-lb/in²
Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S
Thermal Properties
Metric
English
Comments
Melting Point
130
°C
266
°F
Dow Method (DSC)
Crystallization Temperature
118
°C
244
°F
Dow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi)
67.8
°C
154
°F
Molded and tested in accordance with ASTM D4976; ASTM D648
Vicat Softening Point
127
°C
261
°F
ASTM D1525
Brittleness Temperature
<=
-76.1
°C
<=
-105
°F
Molded and tested in accordance with ASTM D4976; ASTM D746
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Dow DMDA-8907 NT 7 High Density Polyethylene Resin
Dow DMDA-8007 NT 7 High Density Polyethylene Resin
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
Chevron Phillips Marlex® 9005 HDPE Injection Molding Resin
Dow DMDA-8904 NT 7 High Density Polyethylene Resin
PDOW1267 / 30485
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.