Asahi Kasei TENAC™-C C84 Copolymer Acetal (POM), Electrically Conductive
Categories:
Polymer
;
Thermoplastic
;
Acetal (Polyoxymethylene, POM)
Material Notes:
Excellent balance of mechanical properties, low friction and wear characteristics. Applications: Automotive parts, electrical & electronic parts, industrial parts.
Information provided by Asahi Kasei Corp.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.38
g/cc
0.0499
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.012
-
0.016
cm/cm
0.012
-
0.016
in/in
Asahi Kasei
Melt Flow
1.0
g/10 min
1.0
g/10 min
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
35.0
MPa
5080
psi
50% RH; ISO 527
Elongation at Break
31 %
31 %
50% RH; ISO 527
Tensile Modulus
2.70
GPa
392
ksi
50% RH; ISO 527
Flexural Modulus
2.60
GPa
377
ksi
50% RH; ISO 178
Charpy Impact, Notched
0.300
J/cm²
1.43
ft-lb/in²
ISO 179
Electrical Properties
Metric
English
Comments
Volume Resistivity
1.0
-
10
ohm-cm
1.0
-
10
ohm-cm
IEC 60093
Surface Resistance
1.0
-
10
ohm
1.0
-
10
ohm
IEC 60093
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
145
°C
293
°F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi)
83.0
°C
181
°F
ISO 75
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Evonik Vestamid® L-R1-MHI Antistatic, Black, Electrically Conductive Nylon 12
A. Schulman ComAlloy E-16903B Nylon 6/6, Electrically Conductive - Stainless Steel Fiber Filled
Asahi Kasei TENAC™-C TFC77 Copolymer Acetal (POM), Electrically Conductive
Asahi Kasei TENAC™-C TFC64 Copolymer Acetal (POM), Electrically Conductive
Precision Polymer Engineering S70L Conductive Silicone Rubber
PASAHI8117 / 221144
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.