MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 1200 T-70A Z NATURAL Ether-based Thermoplastic Polyurethane Elastomer (; Translucent
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 70
@Time 10.0 sec
70
@Time 0.00278 hour
ASTM D 2240
Tensile Strength at Break 21.4 MPa
@Thickness 3.20 mm
3100 psi
@Thickness 0.126 in
Break; Die C; 20 in/min (500 mm/min); ASTM D 412
Tensile Stress at Strain 3.03 MPa
@Strain 100 %,
Thickness 3.20 mm
440 psi
@Strain 100 %,
Thickness 0.126 in
Die C; 20 in/min (500 mm/min); ASTM D 412
Elongation at Break 765 %
@Thickness 3.20 mm
765 %
@Thickness 0.126 in
Die C, 20 in/min (500 mm/min); ASTM D 412
Tear Strength 61.4 kN/m350 pliDie C; ASTM D 624
 
Processing PropertiesMetricEnglishComments
Melt Temperature 188 - 199 °C370 - 390 °F
Mold Temperature 15.6 - 37.8 °C60.0 - 100 °F
Drying Temperature 82.2 - 93.3 °C
@Time 7200 - 14400 sec
180 - 200 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.030 %<= 0.030 %
Dew Point <= -17.8 °C<= 0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Miracll M75 Thermoplastic Polyurethane (TPUR), Polyether Grade
Miracll M70 Thermoplastic Polyurethane (TPUR), Polyether Grade
Huntsman IROGRAN® A 75 P 4665N TPU-Polyether
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer

PQZUA21364 / 134781

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.