MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel CPM® 154 Tool Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Tool Steel

Material Notes: CPM 154 is CPM-manufactured version of Crucible’s standard 154 CM. The CPM manufacturing process produces a uniform distribution of the carbides in this grade, giving this CPM 154 easier grinding and polishing, plus better toughness, than conventional 154 CM, while retaining similar heat treat response and wear properties. CPM 154 offers better corrosion resistance, better wear resistance and better hot-hardness than 440C, plus higher toughness. For knifemakers, it offers better edge retention and chipping resistance than 440C.

Information provided by Crucible Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.78 g/cc0.281 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6262austenitized at 1900°F then quenched
 6363austenitized at 1900°F then quenched + freeze
 51
@Tempering Temp. 566 °C
51
@Tempering Temp. 1050 °F
austenitized at 1900°F then quenched and tempered
 54
@Tempering Temp. 538 °C
54
@Tempering Temp. 1000 °F
austenitized at 1900°F then quenched and tempered
 56
@Tempering Temp. 316 °C
56
@Tempering Temp. 600 °F
austenitized at 1900°F then quenched and tempered
 56
@Tempering Temp. 427 °C
56
@Tempering Temp. 800 °F
austenitized at 1900°F then quenched and tempered
 56
@Tempering Temp. 482 °C
56
@Tempering Temp. 900 °F
austenitized at 1900°F then quenched and tempered
 59
@Tempering Temp. 204 °C
59
@Tempering Temp. 400 °F
austenitized at 1900°F then quenched and tempered
Modulus of Elasticity 207 GPa30000 ksi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  7.02 µm/m-°C
@Temperature -74.0 - 21.0 °C
3.90 µin/in-°F
@Temperature -101 - 69.8 °F
 7.33 µm/m-°C
@Temperature 21.0 - 38.0 °C
4.07 µin/in-°F
@Temperature 69.8 - 100 °F
 10.35 µm/m-°C
@Temperature 21.0 - 149 °C
5.750 µin/in-°F
@Temperature 69.8 - 300 °F
 10.91 µm/m-°C
@Temperature 21.0 - 260 °C
6.061 µin/in-°F
@Temperature 69.8 - 500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.05 %1.05 %
Chromium, Cr 14 %14 %
Iron, Fe 80.95 %80.95 %as balance
Molybdenum, Mo 4.0 %4.0 %
 
Descriptive Properties
Wear Resistance49 mgweight loss, pin abrasion method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
403 Stainless Steel, annealed, sheet
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia
Crucible Steel 154 CM Martensitic Steel
416 Stainless Steel
Crucible Steel CPM® 4V® Tool Steel

NCRUC902 / 160353

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.