MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Monmouth Rubber & Plastics Durafoam™ C19XLDS EPDM  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Special Features:
  • Extremely soft and conforms easily to irregular surfaces
  • Superior buoyancy
  • Excellent chemical resistance
  • 100% free of HCFC & CFC
  • Available in custom colors upon request for quote
  • Compatible with most general purpose adhesives
Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of:
1. Light at 70°C for 8 hours
2. Dark at 50° C for 4 hours
3. Condensation Cooling for 15 minutes

Information provided by Monmouth Rubber & Plastics Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0641 g/cc0.00231 lb/in³
Water Absorption <= 5.0 %<= 5.0 %10% allowed; ASTM D1056
Linear Mold Shrinkage <= 0.017 cm/cm<= 0.017 in/in
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 0.0138 - 0.0345 MPa2.00 - 5.00 psi25% PSI Compression
K Factor (Wear Factor) 0.260.26
 
Descriptive Properties
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lanxess Antilux® 110 Wax
Monmouth Rubber & Plastics Durafoam™ P497SHD Red EPDM
Garlock 563 EPDM Sheet Rubber
E-Polymers EFLEX® V1040 EPDM/TPV
Ethylene Propylene Rubber (EPM, EPDM)

PMONM017 / 160819

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.