MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

80-20 Solder (80Sn-20Pb)
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy; Tin Alloy

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.05 g/cc0.291 lb/in³estimated from similar composition
Viscosity 44400 cP
@Temperature 280 °C
44400 cP
@Temperature 536 °F
Surface Tension 514 dynes/cm
@Temperature 280 °C
514 dynes/cm
@Temperature 536 °F
 
Thermal PropertiesMetricEnglishComments
Melting Point 183 - 199 °C361 - 390 °F
Solidus 183 °C361 °F
Liquidus 199 °C390 °F
 
Component Elements PropertiesMetricEnglishComments
Lead, Pb 20 %20 %
Tin, Sn 80 %80 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
60-40 Soft Solder (60 Sn-40Pb) - ASTM B 32 Grade Sn60
50/50 (50Pb-50Sn) Solder- ASTM B 32 Grade Sn50, UNS L55030
Eutectic Solder (63Sn-37Pb) - ASTM B 32 Grade Sn63
88Pb-10Sn-2Ag Lead-Tin-Silver Solder, ASTM B 32 Grade Sn10B
Tin-Silver Solder (95Sn-5Ag), ASTM B 32 Grade Sn95

MLSS72 / 178196

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.