MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tabriz SD-0150 General Purpose ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: SD0150 is one of the styrenic terpolymer (ABS) grade with improved toughness versus HIPS grades. SD0150 exhibits, low shrinkage, and good dimensional stability. SD0150 is widely used in general injection molding applications. Use this information as a guide to aid you in selecting the proper resin for your application. Applications: Furniture, Automotive Parts ,General Injection Molding, Appliances Casing, Office Supplies. Drying: Drying prior to processing is recommended in a desiccant dehumidifying hopper dryer. An inlet air dew point of -20°F (-29°C) or below is recommended to achieve a moisture content 0.1%. Typical drying conditions are 2 hours at 180° - 190°F (82° - 88°C). Drying for 4 hours at 160° - 170°F (71°-77°C) is also adequate.

Information provided by Tabriz Petrochemical Commercial Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.600 g/cc0.0217 lb/in³
Melt Flow 1.8 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.8 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 44.1 MPa6400 psiASTM D638
Flexural Yield Strength >= 55.9 MPa>= 8110 psiASTM D790
Flexural Modulus >= 1.863 GPa>= 270.2 ksiASTM D790
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ASTM D256
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 98.0 °C
@Load 5.10 kg
208 °F
@Load 11.2 lb
ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced
Lotte Advanced Materials Starex® SD-0150UF ABS, Unreinforced
INEOS Styrolution Terluran® GP-22 ABS
Tabriz SH-0150 Extrusion Grade ABS
Tabriz 5211 EA HDPE

PIPC099 / 48327

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.