MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® AS-20GF/000 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Filler Content 20 %20 %Glass Fiber Reinforcement
Water Absorption 0.050 %0.050 %@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength at Break 70.7 MPa10300 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 6.0 %6.0 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 117 MPa17000 psiASTM D790
Flexural Modulus 3.45 GPa500 ksiASTM D790
Izod Impact, Notched  0.590 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 0.610 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
1.14 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C20.0 µin/in-°FASTM D696
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
@Thickness 3.18 mm
210 °F
@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.1 °C
@Thickness 3.18 mm
196 °F
@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HBHBUL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 249 °C430 - 480 °F
Mold Temperature 65.0 - 85.0 °C149 - 185 °F
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
FormsPellets
Generic MaterialABS
Generic NameAcrylonitrile Butadiene Styrene (ABS)
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS)
Aclo Accutech ABS ABS831G10L Glass Reinforced
Avient Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS)
Avient Edgetek® AS-10GF/000 BLACK Acrylonitrile Butadiene Styrene (ABS)
Aclo Accutech ABS ABS831G20L Glass Reinforced

PH0POL0178 / 144747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.