A polypropylene homopolymer produced by Ineos utilizing unique, catalyst technology. This product is a high flow, controlled-rheology material with a narrow molecular weight distribution. Typical applications include thin-wall, injection molding and compounding. Meets FDA 21CFR 177.1520. |
High flow, controlled-rheology material, narrow molecular weight distribution |