MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kuraray HYBRAR® PH6 Polypropylene Blend
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber; Polypropylene (PP)

Material Notes: Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubber which exhibits high vibration damping properties at room temperatures. Both hydrogenated and non-hydrogenated grades of HYBRAR® are available. In addition to the superior vibration damping properties, hydrogenated grades also exhibit excellent miscibility with polypropylene, and may be used to produce blends with excellent transparency, flexibility and mechanical properties.

A flexible and transparent compound may be obtained by combining a hydrogenated HYBRAR® resin with polypropylene. A homopolymer or random copolymer polypropylene can be used for this application. These compounds have high tensile strength and excellent impact strength. They may be used for film, sheet or profile extrusion applications and make an excellent alternative to flexible PVC.

Mixing Condition: Twin screw extruder @ 210°C

Molding Condition: Press molding @ 210°C

Formulation (parts by weight): Polypropylene (Homopolymer) - 90, HYBRAR® 7311 - 10

Information provided by The Kuraray Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9494
Tensile Strength, Ultimate 34.0 MPa4930 psi
Tensile Modulus 0.380 GPa55.1 ksi
 
Optical PropertiesMetricEnglishComments
Haze 52 %
@Thickness 1.00 mm
52 %
@Thickness 0.0394 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kuraray HYBRAR® HD3 Thermoplastic Rubber-HDPE Blend
Kuraray HYBRAR® Low Rebound Compound # 1
Kuraray HYBRAR® Blends
Kuraray HYBRAR® PP1 Thermoplastic Rubber-Polypropylene Blend
Kuraray HYBRAR® CF1 Mono Layer Cast Film

PKUR062 / 49451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.