MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® 8253 PA6 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/or pigmented versions. Copolymerization results in improved dry as molded toughness and increased flexibility to meet higher impact performance compared to conventional unreinforced homopolymers. Good nylon thermal and chemical properties are maintained along with good strength and stiffness retention.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %24 hour; ISO Test
 8.1 %8.1 %ISO 62
Moisture Absorption at Equilibrium 2.3 %2.3 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM Data; MD
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8282ASTM Test
Tensile Strength at Break 60.0 MPa8700 psi0.2 in/min; ASTM Test
 100 MPa
@Temperature -40.0 °C
14500 psi
@Temperature -40.0 °F
ASTM Test
 100 MPa
@Temperature -40.0 °C
14500 psi
@Temperature -40.0 °F
ISO Data
Tensile Strength, Yield 60.0 MPa8700 psi50mm/min; ISO 527
 65.0 MPa9430 psi2 in/min; ASTM Test
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
ISO Data
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
ASTM Test
 25.0 MPa
@Temperature 80.0 °C
3630 psi
@Temperature 176 °F
ASTM Test
 25.0 MPa
@Temperature 80.0 °C
3630 psi
@Temperature 176 °F
ISO Data
 117 MPa
@Temperature -40.0 °C
17000 psi
@Temperature -40.0 °F
ASTM Test
 117 MPa
@Temperature -40.0 °C
17000 psi
@Temperature -40.0 °F
ISO Data
Elongation at Break 40 %40 %50mm/min, Nominal strain; ISO 527
 >= 100 %>= 100 %2 in/min; ASTM Test
 9.0 %
@Temperature -40.0 °C
9.0 %
@Temperature -40.0 °F
ASTM Test
 9.0 %
@Temperature -40.0 °C
9.0 %
@Temperature -40.0 °F
ISO Data
Elongation at Yield 4.0 %4.0 %50mm/min; ISO 527
 4.0 %4.0 %2 in/min; ASTM Test
 7.0 %
@Temperature -40.0 °C
7.0 %
@Temperature -40.0 °F
ASTM Test
 7.0 %
@Temperature -40.0 °C
7.0 %
@Temperature -40.0 °F
ISO Data
 29 %
@Temperature 80.0 °C
29 %
@Temperature 176 °F
ISO Data
 29 %
@Temperature 80.0 °C
29 %
@Temperature 176 °F
ASTM Test
 34 %
@Temperature 120 °C
34 %
@Temperature 248 °F
ASTM Test
 34 %
@Temperature 120 °C
34 %
@Temperature 248 °F
ISO Data
Tensile Modulus 2.30 GPa334 ksi1mm/min; ISO 527
 0.295 GPa
@Temperature 120 °C
42.8 ksi
@Temperature 248 °F
ISO Data
 0.400 GPa
@Temperature 80.0 °C
58.0 ksi
@Temperature 176 °F
ISO Data
 2.84 GPa
@Temperature -40.0 °C
412 ksi
@Temperature -40.0 °F
ISO Data
Flexural Strength 65.0 MPa9430 psiISO Data
 87.0 MPa12600 psiASTM Test
 14.0 MPa
@Temperature 120 °C
2030 psi
@Temperature 248 °F
ASTM Test
 20.0 MPa
@Temperature 93.0 °C
2900 psi
@Temperature 199 °F
ASTM Test
 25.0 MPa
@Temperature 65.0 °C
3630 psi
@Temperature 149 °F
ASTM Test
 148 MPa
@Temperature -40.0 °C
21500 psi
@Temperature -40.0 °F
ASTM Test
Flexural Modulus 1.90 GPa276 ksiISO Data
 2.21 GPa321 ksiASTM Test
 0.260 GPa
@Temperature 120 °C
37.7 ksi
@Temperature 248 °F
ASTM Test
 0.325 GPa
@Temperature 93.0 °C
47.1 ksi
@Temperature 199 °F
ASTM Test
 0.415 GPa
@Temperature 65.0 °C
60.2 ksi
@Temperature 149 °F
ASTM Test
Izod Impact, Notched 0.800 J/cm
@Temperature -40.0 °C
1.50 ft-lb/in
@Temperature -40.0 °F
ASTM Test
 1.48 J/cm
@Thickness 3.17 mm
2.77 ft-lb/in
@Thickness 0.125 in
ASTM Test
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched 1.80 J/cm²8.57 ft-lb/in²ISO 179
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 99.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
55.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM Test
CTE, linear, Parallel to Flow 88.0 µm/m-°C48.9 µin/in-°FISO 11359
CTE, linear, Transverse to Flow 93.0 µm/m-°C51.7 µin/in-°FISO 11359
Melting Point 220 °C428 °F10 K/min
 220 °C428 °FASTM Test
Deflection Temperature at 0.46 MPa (66 psi) 160 °C320 °FISO 75
 168 °C334 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C131 °FISO 75
 60.0 °C140 °FASTM Test
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FInjection molding
Mold Temperature 70.0 °C158 °FInjection molding
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® 8253 PA6 (Conditioned)
BASF Ultramid® 8350 HS PA6 (Dry)
BASF Ultramid® 8255 HS PA6 (Dry)
BASF Capron® 8351 Impact Modified Nylon 6 (Dry)
BASF Ultramid® 8350 HS BK-102 PA6 (Dry)

PBASF9169 / 84933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.