MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem TR3350UC Random Copolymer Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Description: Maximum see-through clarity, minimal haze; superior color stability, process stability, and gloss; low odor, high melt flow.

Applications: Suggested uses; reusable food containers, housewares, fast-cycle injection molding, packaging. Ultraclear (TM) polypropylene resin offers good clarity and performance, up to 50% improvement in haze over standard clarified products. If offers substitution opportunities versus more expensive resins such as PET, PVC, PC or PS.

Process: Injection Molding

This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by FDA – Food and Drugs Administration. The additives present are covered in appropriate regulation by FDA.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
35 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 31.7 MPa4600 psi2 in/min; ASTM D638
Elongation at Yield 13 %13 %2 in/min; ASTM D638
Flexural Modulus, 1% Secant 1170 MPa170000 psi0.05 in/min; ASTM D-790A
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256A
 
Optical PropertiesMetricEnglishComments
Haze 5.0 %
@Thickness 1.27 mm
5.0 %
@Thickness 0.0500 in
Disc; ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis RF366MO Polypropylene Random Copolymer for Injection Molding
Borealis HD905CF Polypropylene Homopolymer for Cast Film
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Braskem Prisma 2400 RACO Random Polypropylene Copolymer
Braskem TI4020N Impact Copolymer Polypropylene

PBRASK061 / 133699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.