MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Aptek 2313-PMF Hybrid Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.

Production-oriented, snap-cure technology for surface mount applications-allows cure during solder reflow operation. High thixotropy/"tack" strength-holds components with minimal "Z" axis movement during cure. Stable viscosity for over 4 hours at RT-ideal for robotics. Low Tg (<-50°C) for excellent low temperature cycling and performance with minimal stress. Excellent substrate adhesion; superior to silicones: no primer required.

Information provided by Aptek Laboratories, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.00 g/cc0.108 lb/in³ASTM D1475
 
Mechanical PropertiesMetricEnglishComments
Adhesive Bond Strength 2.24 MPa325 psiAl-to-Al Lap Shear; Cured property; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0030 ohm-cm0.0030 ohm-cmCured property; ASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity >= 1.50 W/m-K>= 10.4 BTU-in/hr-ft²-°FCOLORA
Glass Transition Temp, Tg <= -50.0 °C<= -58.0 °FCured property; Perkin Elmer TM-2
Flash Point >= 200 °C>= 392 °FASTM D92
 
Processing PropertiesMetricEnglishComments
Processing Temperature 85.0 °C185 °FCure 120 min.
 125 °C257 °FCure 30 min.
 260 °C500 °FCure 30 sec; through solder reflow process

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CeramTec Rubalit® 708 HP Alumina, 96% (High Performance)
CHT Group SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Ineos Barex® 210 E Acrylonitrile-Methyl Acrylate Copolymer
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity

PAPTEK14 / 24176

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.