MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Precision Polymer Engineering S50E Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Red iron oxide filled, Phenyl Silicone Rubber, 45-55 °IRHD. Silicone rubber having methyl, vinyl and phenyl substituent groups on the polymer chain. To meet UK Ministry of Defence Aerospace Specification DTD818 Class M2. ASTM & ISO designation = PVMQ.

Applications: Excellent heat resistance plus ultra-low temperature flexibility. Used primarily for dry heat static seals. Low physical strength and poor abrasion resistance prevents dynamic sealing. Although silicone will swell in petroleum lubricants, this is not necessarily detrimental in static sealing applications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050°IRHD; ASTM D1415
 6565°IRHD, +15 change after 336 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 3.105 MPa450.3 psi-25% change after 336 hours @ 200°C; ASTM D412
 4.14 MPa600 psiASTM D412
Elongation at Break 50 %50 %-75% change after 336 hours @ 200°C; ASTM D412
 200 %200 %ASTM D412
Compression Set 30 %
@Temperature 100 °C,
Time 252000 sec
30 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -90.0 °C-130 °F
 -90.0 °C-130 °FNon-brittle after 3 minutes
Flash Point >= 300 °C>= 572 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Precision Polymer Engineering S60G Silicone Rubber
Precision Polymer Engineering S60X Silicone Rubber
Precision Polymer Engineering S60S Silicone Rubber
Precision Polymer Engineering S60A Silicone Rubber
Precision Polymer Engineering S50R Silicone Rubber

PPRECI232 / 57956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.