MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100)
Categories: Metal; Ferrous Metal; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese and nitrogen additions are partial substitutes for nickel making them more economical alloys. Because they possess a very desirable combination of economy plus good mechanical properties and corrosion resistance properties, they have been used in a wide variety of consumer and transportation applications.

Balancing of alloying elements (austenitizers versus feritizer) in Type 201 produces an austenitic structure in the annealed condition even at subzero temperatures. This austenitic structure achieves significant strengthening through cold working of the material to produce the transformation to a stronger martensitic structure. Because of its high work hardening rate, it exhibits a high uniform elongation for improved stretchability for severe forming applications such as washing machine baskets.

Typical applications for Types 201 and 201L are cookware bodies/lids, hose clamps, piston rings, transit car structural member, transit car roofing/siding, thermal window spacers, air bag containers, and truck trailer posts and door frames.

Information provided by Allegheny Ludlum Corporation.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.86 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  85
@Temperature 23.0 °C
85
@Temperature 73.4 °F
 85
@Temperature 23.0 °C
85
@Temperature 73.4 °F
Tensile Strength, Ultimate  685 MPa
@Temperature 23.0 °C
99400 psi
@Temperature 73.4 °F
 696 MPa
@Temperature 23.0 °C
101000 psi
@Temperature 73.4 °F
Tensile Strength, Yield  292 MPa
@Temperature 23.0 °C
42400 psi
@Temperature 73.4 °F
 301 MPa
@Temperature 23.0 °C
43700 psi
@Temperature 73.4 °F
Elongation at Break  56 %
@Temperature 23.0 °C
56 %
@Temperature 73.4 °F
 62.5 %
@Temperature 23.0 °C
62.5 %
@Temperature 73.4 °F
Modulus of Elasticity 207 GPa30000 ksi
Compressive Yield Strength 365 MPa52900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000670 ohm-cm0.0000670 ohm-cm
Magnetic Permeability 1.0041.004D.C. Permeability (m at 200 H)
 
Thermal PropertiesMetricEnglishComments
CTE, linear  16.6 µm/m-°C
@Temperature 20.0 - 100 °C
9.22 µin/in-°F
@Temperature 68.0 - 212 °F
 18.0 µm/m-°C
@Temperature 20.0 - 316 °C
10.0 µin/in-°F
@Temperature 68.0 - 601 °F
 18.0 µm/m-°C
@Temperature 20.0 - 358 °C
10.0 µin/in-°F
@Temperature 68.0 - 676 °F
 20.3 µm/m-°C
@Temperature 20.0 - 871 °C
11.3 µin/in-°F
@Temperature 68.0 - 1600 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.3 W/m-K
@Temperature 100 °C
113 BTU-in/hr-ft²-°F
@Temperature 212 °F
 23.0 W/m-K
@Temperature 500 °C
160 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1455 °C2550 - 2651 °F
Solidus 1400 °C2550 °F
Liquidus 1455 °C2651 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 16 - 18 %16 - 18 %
Iron, Fe 72 %72 %as balance
Manganese, Mn 5.5 - 7.5 %5.5 - 7.5 %
Nickel, Ni 3.5 - 5.5 %3.5 - 5.5 %
Nitrogen, N <= 0.25 %<= 0.25 %
Silicon, Si <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100)
AK Steel 201 Austenitic Stainless steel
Outokumpu 4372 Cr-Ni Austenitic Stainless Steel
202 Stainless Steel, Annealed Bar
ATI Allegheny Ludlum Stainless Steel Type 201, 5% Cold Work (UNS S20100)

NL2010 / 17808

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.