MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Flexible A80U0 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Recommended for interior applications.

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.019 cm/cm0.015 - 0.019 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 707015 sec; ASTM D2240
 8080ASTM D2240
Tensile Strength at Break 14.1 MPa2050 psi510 mm/min; ASTM D638
Tensile Stress at Strain 6.21 MPa
@Strain 100 %
901 psi
@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 450 %450 %510 mm/min; ASTM D638
Tear Strength 57.8 kN/m330 pliDie C, 510 mm/min; ASTM D624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.176 GPa25.5 ksiASTM D1043
 0.310 GPa
@Temperature -42.0 °C
45.0 ksi
@Temperature -43.6 °F
ASTM D1043
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -45.0 °C-49.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %
@Thickness 1.91 mm
4.0 %
@Thickness 0.0750 in
ASTM D1003
Transmission, Visible 82 %
@Thickness 1.91 mm
82 %
@Thickness 0.0750 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 174 - 179 °C345 - 354 °F
 193 - 204 °C379 - 399 °F
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Gloss
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Flexible A75G0 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible D6500 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible D8000 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible P484 Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Flexible R7426A Polyvinyl Chloride, Flexible

PH0POL0065 / 144634

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.