MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Saflex® RB11 Clear PVB interlayer
Categories: Polymer; Film

Material Notes: Saflex® Clear PVB interlayer, our most popular formulation, is available in two different adhesion levels for architectural applications. These different adhesion levels are generally selected based on the laminator’s processing parameters. Both formulations give architects and builders the ability to meet or exceed the human safety impact requirements for laminated safety glass with properly produced laminates.
  • Protects building occupants and pedestrians from flying and falling glass shards after accidental breakage
  • Provides security through burglary and forced-entry resistance and ballistics and bomb blast protection
  • Provides severe windstorm and debris-impact resistance
  • Reduces the transmission of unwanted sound into a building’s environment or between walls
Applications:
Interior: Partitions, doors, windows, skylights, furniture, balustrades, retail shelving, flooring
Exterior: Doors, windows, curtain walls, wall coverings, and overhead glazing

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252Cut/stacked to 12.5 mm; ASTM D2240
Tensile Strength at Break 25.0 MPa3630 psiISO 527-3
Elongation at Break 266 %266 %ISO 527-3
Modulus of Elasticity 0.0420 GPa6.09 ksi3 sec
Poissons Ratio 0.500.5050% RH; ASTM D638
Shear Modulus 0.0140 GPa2.03 ksi3 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 155 µm/m-°C
@Temperature 30.0 - 100 °C
86.1 µin/in-°F
@Temperature 86.0 - 212 °F
ASTM D831
Specific Heat Capacity 1.98 J/g-°C
@Temperature 50.0 °C
0.473 BTU/lb-°F
@Temperature 122 °F
ASTM E1269
Thermal Conductivity 0.200 W/m-K
@Temperature 65.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 149 °F
ASTM F433
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4781.478ASTM D542
Haze <= 1.0 %
@Thickness 3.00 mm
<= 1.0 %
@Thickness 0.118 in
clear; ASTM D1003
Yellow Index <= 1.0 %<= 1.0 %3-mm clear; ASTM E313
Transmission, Visible 72 %72 %Solar, 3-mm clear; NFRC 300, ISO 9050, EN410
 89 %89 %Visible, 3-mm clear; NFRC 300, ISO 9050, EN410
 
Descriptive Properties
ColorClear
UV screening>99%300-380 nm, 3-mm clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Saflex® 0.060 inch Clear Protective Interlayer PVB Film for Glass Laminates
Eastman XIR 70.48 Film
Sorbothane Polyurethane Damping Material, 50 Durometer
Eastman Saflex® 1/8" - 0.090" Saflex® - 1/8"
Eastman Vanceva® Polyvinyl Butyral Interlayer

PEATM5025 / 222219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.