MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BNZ Materials Marinite® C Ceramic Board for Aluminum Contact
Categories: Ceramic; Oxide

Material Notes: These boards are heat treated formulations for use in conveying, containing and forming molten aluminum and other non-ferrous metals. Applications include holding furnace linings, tips for continuous casters, transition plates, rings, plugs, baffles, troughs, spouts, floats and filter boxes.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.865 g/cc0.0312 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture 0.00620 GPa0.899 ksi
Compressive Yield Strength 11.0 MPa
@Strain 5.0 %
1600 psi
@Strain 5.0 %
Compressive Strength 15.2 MPa2200 psiultimate load
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity  0.140 W/m-K
@Temperature 204 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 399 °F
 0.140 W/m-K
@Temperature 316 °C
0.972 BTU-in/hr-ft²-°F
@Temperature 601 °F
 0.150 W/m-K
@Temperature 427 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 801 °F
 0.150 W/m-K
@Temperature 538 °C
1.04 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Shrinkage  2.3 %
@Temperature 732 °C,
Time 86400 sec
2.3 %
@Temperature 1350 °F,
Time 24.0 hour
Length/width, Soaking Heat Changes
 9.4 %
@Temperature 732 °C,
Time 86400 sec
9.4 %
@Temperature 1350 °F,
Time 24.0 hour
Thickness, Soaking Heat Changes
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 2.5 %2.5 %
Loss on Ignition(%) 5.8 %
@Temperature 732 °C
5.8 %
@Temperature 1350 °F
 
Descriptive Properties
Screw Holding Strength100 kgat 7/8" penetration

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chosun Refractories PT-170 Plastic Refractory
Anderman Ceramics EZC96P Zirconia, 96%, Calcia-Stabilized
Sharadaa Ceramics Calcium Silicate Block
Sharadaa Ceramics REFCAST C High Alumina Castables
Sharadaa Ceramics REFINSUL ZAP-014 Insulating Castables

CBNZ929 / 149169

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.