MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4646
Tensile Strength 7.398 MPa1073 psi
Elongation at Break 530 %530 %
100% Modulus 0.972 MPa
@Strain 100 %
141 psi
@Strain 100 %
200% Modulus 1.30 MPa
@Strain 200 %
189 psi
@Strain 200 %
300% Modulus 1.70 MPa
@Strain 300 %
247 psi
@Strain 300 %
Tear Strength 12.1 kN/m69.0 pliDie C
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 149 °C
0.167 hour
@Temperature 300 °F
 
Descriptive Properties
Formulation as Tested0.2Stearic Acid
 0.25Irganox 1010
 0.25Tinuvin 328
 0.25Tinuvin 765
 0.3Silquest A-172
 0.5Luperox 231
 100Millathane 97
 15Wacker HDK-N20
 15Mediaplast NB-4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-326 (HS-HAF)
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
Northstar Polymers MPC-W44A Polyurethane Gel
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR MBT
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Carbon Black, N-220 (ISAF)

PMILL124 / 87168

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.