MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Iupital® FC2020D Copolymer Acetal
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Carbon Fiber Filled

Material Notes: Electro conductive, carbon fiber 20%. Reinforced filled 1. Iupital is a copolymer-type acetal resin produced with our proprietary manufacturing process. Used in a wide range of industries, Iupital is ideal for precision machinery, automobile, OA and electronics applications. Well-balanced mechanical properties and high fatigue resistance. Excellent anticreep properties. Excellent low friction and anti-wear properties. Wide range of operating temperatures. High oil and organic chemical resistance. Excellent thermal stability in molding.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183
Moisture Absorption 0.360 %
@Temperature 23.0 °C
0.360 %
@Temperature 73.4 °F
60% RH
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 3.00 mm
0.0040 in/in
@Thickness 0.118 in
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527-1,2
Elongation at Break 1.5 %1.5 %ISO 527-1,2
Tensile Modulus 17.0 GPa2470 ksiISO 527-1,2
Flexural Strength 200 MPa29000 psiISO 178
Flexural Modulus 16.0 GPa2320 ksiISO 178
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179-1,2
Charpy Impact, Notched 0.450 J/cm²2.14 ft-lb/in²ISO 179-1,2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 200 ohm-cm200 ohm-cmIEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 166 °C331 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 164 °C327 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 162 °C324 °FISO 75-1,2
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celstran® PP-GF60-25 AD3002 Black PP, 60% Glass Reinforced
RTP Company RTP 1379 Polyphenylene Sulfide (PPS), Glass Fiber - Mineral
BASF Ultradur® B 4040 G10 BK5110 50% Glass Filled PBT
BASF Petra® 140 45% Glass Filled PET
Celanese FORTRON 6160B4 PPS, 60% Mineral / Glass Reinforced

PMITSU9149 / 191822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.