MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese SO.F.TER Forprene® 6NE.A75 Extrusion Grade TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Forprene is a Vulcanized Thermoplastic Elastomer. Applications include automotive (air ducts, pipe grommets, weather seals, glass encapsulation, belt line seals, air vents, buttons, mats, suspension bellows), building (extruded seals for doors and windows, simple or co-molded hydraulic seals), household appliances (anti-vibration mounts, inlet pipes and exhaust manifolds, seals, drum suspension bushes, shock absorbers), Tools (handles and grips), Electrical equipment (sheaths for condensers, plugs and loose sockets, special cables requiring good electrical insulation properties, UV-resistance, good thermal resistance and low specific gravity), and Miscellaneous (wheels, drive belts, high/low pressure pipes, mats for motor scooters, O-rings).

Information provided by SO.F.TER. Spa

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ASTM D 792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7676ASTM D 2240
Tensile Strength 7.40 MPa1070 psiASTM D412 C
Elongation at Break 560 %560 %ASTM D412-C
100% Modulus 2.80 MPa
@Strain 100 %
406 psi
@Strain 100 %
ASTM D412 C
Tear Strength 33.0 kN/m188 pliASTM D624 C
Compression Set 39 %
@Temperature 70.0 °C,
Time 79200 sec
39 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese SO.F.TER Forprene® 6NE.A80 Extrusion Grade TPE
Celanese SO.F.TER Forprene® 6NE.A65 Extrusion Grade TPE
Celanese SO.F.TER Forprene® 6NE.A85 Extrusion Grade TPE
Celanese SO.F.TER Forprene® 6NM.A80 TPE
Celanese SO.F.TER Forprene® 6NM.A85 TPE

PSOFS686 / 162150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.