MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Azoty Tarnow™ Tarnamid® T-27 MSK NYLON 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Nucleated

Material Notes: Fast cycling grade with addition of nucleating and slip agent

Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 1.8 %1.8 %23°C/24 hr; ISO 62
Linear Mold Shrinkage 0.018 cm/cm0.018 in/in60x60x2; ISO 294-4
Melt Flow 100 g/10 min
@Load 5.00 kg,
Temperature 275 °C
100 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 74.0 MPa10700 psiConditioned; ISO 2039-1
 150 MPa21800 psiDry, 358 N; ISO 2039-1
Tensile Strength, Yield 45.0 MPa6530 psiConditioned; ISO 527
 85.0 MPa12300 psiDry; ISO 527
Elongation at Break 50 %50 %Dry; ISO 527
 200 %200 %Conditioned; ISO 527
Tensile Modulus 1.30 GPa189 ksiConditioned, 1mm/min; ISO 527
 3.50 GPa508 ksiDry; ISO 527
Izod Impact, Notched (ISO) 4.50 kJ/m²2.14 ft-lb/in²Dry, 1A; ISO 180
 NBNBConditioned; ISO 180
Charpy Impact, Notched NBNBConditioned; ISO 179
 NBNBDry, 1eA; ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmConditioned; ISO 60093
 1.00e+15 ohm-cm1.00e+15 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmConditioned; ISO 60093
 1.00e+15 ohm1.00e+15 ohmDry; IEC 60093
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Comparative Tracking Index 600 V600 VIEC 112
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °F10°C/min.; ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C122 °FConditioned; ISO 75
 60.0 °C140 °FDry; ISO 75
Vicat Softening Point 200 °C392 °F50 N; ISO 306
Flammability, UL94 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
Glow Wire Test 750 °C
@Thickness 2.00 mm
1380 °F
@Thickness 0.0787 in
PN-EN-60695-21
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 290 °C446 - 554 °F
Mold Temperature 75.0 - 120 °C167 - 248 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Azoty Tarnow™ Tarnamid® T-27 MRS NYLON 6
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced

PZAK059 / 72898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.