Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. Exceed 1018EB contains slip agent and antiblock, which makes it suitable for formulations which require good openability and a low friction coefficient. It is a ready-to-use versatile polymer for demanding mono layer and multi layer blown film applications. Availability: Africa & Middle East and Europe Additive: - Antiblock: 2500 ppm
- Slip: 750 ppm
- Processing Aid: Yes
- Thermal Stabilizer: Yes
Applications:- Agricultural Film
- Bag in a Box
- Barrier Food Packaging
- Blown Film
- Bread Bags
- Food packaging
- Form Fill and Seal Packaging
- Freezer Film
- General Packaging
- Heavy Duty Bags
- Lamination Film
- Multilayer Packaging Film
- Overwrap Film
- Packaging Films
- Premium Trash Bags
- Stand Up Pouches
- Trash Bags
Information provided by ExxonMobil |