MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales
metalmen Is Your Direct to US Manufacturing Source for High Purity Metals

Cobalt, Co
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Pure Element

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.80 g/cc0.318 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 58.93320158.9332011995
Atomic Number 2727
Thermal Neutron Cross Section 34.8 barns/atom34.8 barns/atom
X-ray Absorption Edge 1.608 Å1.608 ÅK
 13.343 Å13.343 ÅLI
 15.534 Å15.534 ÅLII
 15.8314 Å15.8314 ÅLIII
Electrode Potential -0.280 V-0.280 V
Electronegativity 1.881.88Pauling
Ionic Radius 0.630 Å0.630 ÅCrystal Ionic Radius for Valence +3
 0.720 Å0.720 ÅCrystal Ionic Radius for Valence +2
Electrochemical Equivalent 1.1 g/A/h1.1 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 125125
Hardness, Vickers 253253
Tensile Strength, Yield 225 MPa32600 psi
Modulus of Elasticity 211 GPa30600 ksi
Poissons Ratio 0.320.32
Shear Modulus 82.6 GPa12000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000624 ohm-cm0.00000624 ohm-cm
Magnetic Permeability 6868Initial
 <= 245<= 245
Curie Temperature 1121 °C2050 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 259.6 J/g111.7 BTU/lb
Heat of Vaporization 3280 J/g1410 BTU/lb
CTE, linear  12.5 µm/m-°C
@Temperature 20.0 - 100 °C
6.94 µin/in-°F
@Temperature 68.0 - 212 °F
 14.2 µm/m-°C
@Temperature 200 °C
7.89 µin/in-°F
@Temperature 392 °F
Specific Heat Capacity 0.440 J/g-°C0.105 BTU/lb-°F
Thermal Conductivity 69.21 W/m-K480.3 BTU-in/hr-ft²-°F
Melting Point 1493 °C2719 °F
Boiling Point 2927 °C5301 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.13
@Temperature 500 °C
0.13
@Temperature 932 °F
unoxidized, total spectrum
Reflection Coefficient, Visible (0-1) 0.370.37200 nm
 0.6750.6751060 nm
 
Component Elements PropertiesMetricEnglishComments
Cobalt, Co 100 %100 %
 
Descriptive Properties
CAS Number7440-48-4

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Iron, Fe
Aluminum, Al
Nickel, Ni
Molybdenum, Mo, Annealed
Chromium, Cr; Recrystallized

AMECo00 / 23

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.