MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Steels, General Properties
Categories: Metal

Material Notes: Steel compositions vary widely. Steels in general have a lower carbon content than cast irons, and lower amounts of impurities like phosphorus and sulfur. The composition chart above represents typical ranges for basic steel constituents. Other alloying elements such as Boron, Chromium, Cobalt, Columbium (Niobium), Copper, Molybdenum, Nickel, Nitrogen, Selenium, Tantalum, Titanium, Tungsten, and Vanadium are added to improve corrosion, high temperature, and mechanical properties of steel. The properties listed below reflect typical properties for Steels. In general, properties such as density, thermal conductivity, and electrical resistivity do not vary greatly with composition or heat treatment, whereas properties such as tensile strength, elongation, and hardness are highly dependent on composition and heat treatment.

Key Words: carbon steels, alloy steels
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 - 8.00 g/cc0.282 - 0.289 lb/in³Density usually ranges from 7.8 - 7.9 g/cc for carbon and low alloy steels. Stainless steels typically have densities around 8 g/cc.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 121121Varies widely with composition and heat treatment.
Hardness, Knoop 140140Varies widely with composition and heat treatment.
Hardness, Vickers 126126Varies widely with composition and heat treatment.
Tensile Strength, Ultimate 420 MPa60900 psiThis is the value for AISI 1020, a mild steel. Values can range from 295 - 2400 MPa, depending on composition and heat treatment.
Tensile Strength, Yield 350 MPa50800 psiAISI 1020 Steel. Yield strength varies as Ultimate Tensile Strength values, from 200 - 2100 MPa.
Elongation at Break 15 %15 %AISI 1020. Generally as hardness and tensile strength goes up, elongation goes down.
Modulus of Elasticity 200 GPa29000 ksi
Bulk Modulus 140 GPa20300 ksi
Poissons Ratio 0.250.25Calculated
Machinability 65 %65 %for 1020 steel. Varies from 0 - 100, Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPa11600 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.50 - 12.6 µm/m-°C
@Temperature 20.0 °C
5.28 - 7.00 µin/in-°F
@Temperature 68.0 °F
steels generally range between 9.5-12.6 µm/m°C
 11.7 µm/m-°C
@Temperature 0.000 - 250 °C
6.50 µin/in-°F
@Temperature 32.0 - 482 °F
average
 12.8 µm/m-°C
@Temperature 0.000 - 500 °C
7.11 µin/in-°F
@Temperature 32.0 - 932 °F
average
 13.9 µm/m-°C
@Temperature 0.000 - 1000 °C
7.72 µin/in-°F
@Temperature 32.0 - 1830 °F
average
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°F
Thermal Conductivity 44.0 - 52.0 W/m-K305 - 361 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.030 - 1.25 %0.030 - 1.25 %
Iron, Fe 80 - 98 %80 - 98 %
Manganese, Mn 0.20 - 16 %0.20 - 16 %
Phosphorus, P <= 0.050 %<= 0.050 %
Silicon, Si 0.00 - 0.50 %0.00 - 0.50 %
Sulfur, S <= 0.050 %<= 0.050 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Carbon Steel
G-10 Fiberglass Epoxy Laminate Sheet
Overview of materials for AISI 1000 Series Steel
Overview of materials for Medium Carbon Steel
304 Stainless Steel

MS0001 / 13909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.