MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Lacqtene® 6002 FLG 42 HDPE film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability.

LACQTENE® 6002 FLG 42 has been especially dedicated to film applications where a lower gel content and a higher rigidity are required, particularly in blend and coextrusion with LLDPE and LDPE.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D 792
Melt Flow 0.20 g/10 min
@Load 2.16 kg
ISO 1133
 0.80 g/10 min
@Load 5.00 kg
ISO 1133
High Load Melt Index 16.5 g/10 min
@Load 21.6 kg
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 32.0 MPaISO R527
Elongation at Break 830 %ISO R527
Flexural Modulus 0.850 GPa
Dart Drop Test 65.0 gASTM D 1709 A
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °CISO 11357-3
Vicat Softening Point 121 °CISO 306
 
Optical PropertiesOriginal ValueComments
Haze 55 %ASTM D 1003
Gloss 10 %45 degrees; ASTM D 2457
 
Descriptive Properties
Food StatusFormulated to comply with most requirements of food packaging regulations

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Reliance Industries Relene E52009 Polyethylene
Total HT 514 MDPE film
Kazanorgsintez 293-285SK High Density Polyethylene Composite, Film Grade
Kazanorgsintez 293-285D High Density Polyethylene Composite, Film Grade

PFINAP105 / 38688

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.