MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivity useful in many electronic applications. It is a soft 100% solids thixotropic paste provided in a 1:1 ratio. It is recommended to mix by weight but extrusion of equal length beads from syringes is commonly used as a method of measurement as small quantities are commonly used. It also can be packaged in small side-by-side dispensing cartridges for use with static mixers. This system is also available in a pre-mix and frozen format. SEC1233 provides exceptionally high conductivity starting immediately after mixing and improves as the curing process proceeds. It also has the additional benefit of very high thermal conductivity due to its high silver loading. It gives good environmental protection while having tenacious adhesion to various metals and other common assembly materials.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.90 g/ccMixed; TM R050-16
Water Absorption <= 0.20 %
@Time 86400 sec
TM R050-35
Viscosity 582000 cP
@Shear Rate 1.00 1/s
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70
Tensile Strength at Break 400 psiTM R050-36
Tensile Strength, Ultimate 450 psiTM R050-36
Tensile Strength, Yield 450 psiTM R050-36
Elongation at Break 20 - 30 %TM R050-36
Tensile Modulus 10.0 ksiTM R050-36
Compressive Yield Strength 2000 psiTM R050-38
Compressive Strength 7500 psiUltimate; TM R050-38
 7500 psiBreak; TM R050-38
Compressive Modulus 11.0 ksiTM R050-38
Adhesive Bond Strength 600 psiLap Shear-Aluminum
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0016 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°C
@Temperature <=10.0 °C
Below Tg
Thermal Conductivity 4.60 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 10.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 60.0 °C
 24.0 - 72.0 hour
@Temperature 25.0 °C
Pot Life >= 240 min
 
Descriptive Properties
Appearancesilver paste
Mix Ratio by Volume1:1
Side-By-Side Cartridges CapableYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Abatron 8602-2 A/B Carbon-Filled Electrically Conductive Epoxy Compound
Resinlab® EP1200LV Casting Resin
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab® EP1290 Clear Mineral Filled Epoxy Adhesive

PRESL172 / 101586

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.