MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1) Annealed 8 hr at 790°C (1450°F)
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Information provided by Allvac and the references.

Characteristics: Low density, high modulus, high stiffness/density ratio, moderate to high strength, good elevated temperature tensile properties and excellent creep resistance (for operating temperatures up to 455°C)

Applications: Fan & compressor blades, discs, spacers, seals, rings.

Forms typically available: Billet, bar, rod, extrusions, plate, sheet and wire.

5 other heat treatments of this alloy are in MatWeb.

Key Words: Ti8Al1Mo1V, UNS R54810; Ti-811
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.37 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 334Estimated from Rockwell C.
Hardness, Knoop 363Estimated from Rockwell C.
Hardness, Rockwell C 36
Hardness, Vickers 349Estimated from Rockwell C.
Tensile Strength 689 MPa
@Temperature 427 °C
Tensile Strength, Ultimate 1000 MPa
Tensile Strength, Yield 930 MPa
Elongation at Break 12 %
Creep Strength 620 MPa
@Temperature 316 °C,
Time >=3.60e+6 sec
strain 0.2%
Rupture Strength 276 MPa
@Temperature 538 °C,
Time 3.60e+6 sec
Tensile Modulus 121 GPa
Modulus of Rigidity 46.2 GPa
Compressive Yield Strength 980 MPa
Compressive Modulus 124 GPa
Notched Tensile Strength 1100 MPaKt (stress concentration factor) = 6.0
Ultimate Bearing Strength 2000 MPae/D = 2
Bearing Yield Strength 1480 MPae/D = 2
Poissons Ratio 0.32
Fatigue Strength 170 MPa
@# of Cycles 1.00e+7
Kt (stress concentration factor) = 2.6
 340 MPa
@# of Cycles 1.00e+7
unnotched
 725 MPa
@# of Cycles 50000
unnotched
Fracture Toughness 910 MPa-m½
Shear Modulus 46.0 GPa
Shear Strength 620 MPaUltimate shear strength
Charpy Impact 20.0 - 30.0 JV-notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.50 µm/m-°C
@Temperature 20.0 °C
Annealed
 9.20 µm/m-°C
@Temperature 250 °C
Specific Heat Capacity 0.502 J/g-°C
Thermal Conductivity 6.00 W/m-K
Melting Point <= 1540 °C
Liquidus 1540 °C
Beta Transus 1038 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 7.35 - 8.35 %
Carbon, C <= 0.080 %
Hydrogen, H <= 0.015 %
Iron, Fe <= 0.30 %
Molybdenum, Mo 0.75 - 1.25 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.40 %
Oxygen, O <= 0.12 %
Titanium, Ti 88.185 - 91.15 %As Balance; Elemental Composition per ASTM B265
Vanadium, V 0.75 - 1.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1)
304 Stainless Steel (UNS S30400); Annealed Plate
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1) Duplex Anneal
410 Stainless Steel

MTA816 / 14141

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.