MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polytrimethylene Terephthalate (PTT)

Material Notes: 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate

Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength stif

Information provided by DuPont.

Key Words: PTT-GF30
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Water Absorption at Saturation 0.080 %Immersion 24h; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cmISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cmISO 294-4 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 165 MPaISO 527-1/-2
Tensile Stress at Strain 11.336 MPa
@Strain 0.3 %,
Temperature 150 °C
ISO 11403-1 -2
 20.97 MPa
@Strain 0.2 %,
Temperature 0.000 °C
ISO 11403-1 -2
 23.336 MPa
@Strain 0.7 %,
Temperature 150 °C
ISO 11403-1 -2
 30.288 MPa
@Strain 1 %,
Temperature 150 °C
ISO 11403-1 -2
 35.588 MPa
@Strain 1.3 %,
Temperature 150 °C
ISO 11403-1 -2
 41.122 MPa
@Strain 0.4 %,
Temperature 23.0 °C
ISO 11403-1 -2
 44.834 MPa
@Strain 0.5 %,
Temperature 40.0 °C
ISO 11403-1 -2
 60.665 MPa
@Strain 0.6 %,
Temperature 0.000 °C
ISO 11403-1 -2
 67.258 MPa
@Strain 0.8 %,
Temperature 40.0 °C
ISO 11403-1 -2
 73.007 MPa
@Strain 0.7 %,
Temperature -40.0 °C
ISO 11403-1 -2
 86.656 MPa
@Strain 0.9 %,
Temperature 23.0 °C
ISO 11403-1 -2
 87.009 MPa
@Strain 1.1 %,
Temperature 40.0 °C
ISO 11403-1 -2
 87.947 MPa
@Strain 0.9 %,
Temperature 0.000 °C
ISO 11403-1 -2
 99.975 MPa
@Strain 1 %,
Temperature -40.0 °C
ISO 11403-1 -2
 103.52 MPa
@Strain 1.4 %,
Temperature 40.0 °C
ISO 11403-1 -2
 110.48 MPa
@Strain 1.2 %,
Temperature 23.0 °C
ISO 11403-1 -2
 112.39 MPa
@Strain 1.2 %,
Temperature 0.000 °C
ISO 11403-1 -2
 124.61 MPa
@Strain 1.3 %,
Temperature -40.0 °C
ISO 11403-1 -2
 130.43 MPa
@Strain 1.5 %,
Temperature 23.0 °C
ISO 11403-1 -2
 147.73 MPa
@Strain 1.6 %,
Temperature -40.0 °C
ISO 11403-1 -2
Elongation at Break 2.5 %ISO 527-1/-2
Tensile Modulus 11000 MPaISO 527-1/-2
Flexural Strength 245 MPaISO 178
Flexural Modulus 9600 MPaISO 178
Secant Modulus 3.19 GPa
@Strain 1.9 %,
Temperature 100 °C
ISO 11403-1 -2
 3.20 GPa
@Strain 2.4 %,
Temperature 80.0 °C
ISO 11403-1 -2
 3.71 GPa
@Strain 1.3 %,
Temperature 100 °C
ISO 11403-1 -2
 3.84 GPa
@Strain 1.6 %,
Temperature 80.0 °C
ISO 11403-1 -2
 4.16 GPa
@Strain 0.9 %,
Temperature 100 °C
ISO 11403-1 -2
 4.51 GPa
@Strain 0.9 %,
Temperature 80.0 °C
ISO 11403-1 -2
 4.7482 GPa
@Strain 0.5 %,
Temperature 100 °C
ISO 11403-1 -2
 5.0068 GPa
@Strain 0.5 %,
Temperature 80.0 °C
ISO 11403-1 -2
 5.4921 GPa
@Strain 0.1 %,
Temperature 100 °C
ISO 11403-1 -2
 5.565 GPa
@Strain 0.1 %,
Temperature 80.0 °C
ISO 11403-1 -2
 6.54 GPa
@Strain 1.9 %,
Temperature 40.0 °C
ISO 11403-1 -2
 7.22 GPa
@Strain 1.5 %,
Temperature 40.0 °C
ISO 11403-1 -2
 7.661 GPa
@Strain 2 %,
Temperature 23.0 °C
ISO 11403-1 -2
 7.91 GPa
@Strain 1.1 %,
Temperature 40.0 °C
ISO 11403-1 -2
 8.50 GPa
@Strain 1.8 %,
Temperature 0.000 °C
ISO 11403-1 -2
 8.51 GPa
@Strain 1.6 %,
Temperature 23.0 °C
ISO 11403-1 -2
 8.57 GPa
@Strain 0.7 %,
Temperature 40.0 °C
ISO 11403-1 -2
 8.59 GPa
@Strain 2.1 %,
Temperature -40.0 °C
ISO 11403-1 -2
 9.11 GPa
@Strain 1.7 %,
Temperature -40.0 °C
ISO 11403-1 -2
 9.21 GPa
@Strain 1.2 %,
Temperature 23.0 °C
ISO 11403-1 -2
 9.23 GPa
@Strain 1.3 %,
Temperature 0.000 °C
ISO 11403-1 -2
 9.32 GPa
@Strain 0.1 %,
Temperature 40.0 °C
ISO 11403-1 -2
 9.59 GPa
@Strain 1.3 %,
Temperature -40.0 °C
ISO 11403-1 -2
 9.77 GPa
@Strain 0.9 %,
Temperature 0.000 °C
ISO 11403-1 -2
 9.98 GPa
@Strain 0.7 %,
Temperature 23.0 °C
ISO 11403-1 -2
 10.1 GPa
@Strain 0.9 %,
Temperature -40.0 °C
ISO 11403-1 -2
 10.3 GPa
@Strain 0.5 %,
Temperature 0.000 °C
ISO 11403-1 -2
 10.45 GPa
@Strain 0.1 %,
Temperature 23.0 °C
ISO 11403-1 -2
 10.59 GPa
@Strain 0.1 %,
Temperature 0.000 °C
ISO 11403-1 -2
 11.022 GPa
@Strain 0.1 %,
Temperature -40.0 °C
ISO 11403-1 -2
Charpy Impact Unnotched 50.0 kJ/m²ISO 179/1eU
 45.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 8.00e+13 ohmIEC 60093
Dielectric Constant 4.0
@Frequency 1e+6 Hz
IEC 60250
 4.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 38.0 kV/mmIEC 60243-1
Dissipation Factor 0.0012
@Frequency 100 Hz
IEC 60250
 0.0155
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 300 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 7.00 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 83.0 µm/m-°CISO 11359-1/-2
Melting Point 227 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 226 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
 HB
@Thickness 0.800 mm
IEC 60695-11-10
Oxygen Index 20 %ISO 4589-1/-2
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PTT-GF30<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPTT-GF30
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FKuR Kunststoff Bio-Flex® S 6540 Compostable PLA Blend
Biomer P240 PHB Biodegradable Polymer
BASF Ecovio® C2203 F Blend Biodegradable Polyester
DuPont Mobility and Materials Sorona® 3015GV BK001 Polytrimethylene Terephthalate (PTT)
DuPont Mobility and Materials Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT)

PZDSY5297 / 161124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.