MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lord Adhesives Versilok® 271/331 Acrylic Adhesive System
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD Versilok® 271/331 adhesive is a two-component, epoxy-modified acrylic adhesive used to bond a variety of automotive sheet metals, including hot-dip galvanized, electro-galvanized, bare aluminum, and cold rolled steel. Versilok 271/331 adhesive can be either room temperature cured or heat cured for faster processing. Glass beads are included in the adhesive system providing a mechanical lock between substrates. Versilok 271/331 adhesive also contains an odor suppressant. Versilok 271/331 adhesive is approved by Chrysler (MS-CD-500).

Features: contains glass beads which provide a mechanical lock that will prevent shifting of substrate panels. utilizes non-sagging rheology; replaces the need for spot welding which degrades metal and allows rusting to occur. develops a high strength bond in less than one hour at room temperature, eliminating metal warpage caused by high curing induction temperatures. Induction heating should be conducted at 110°C (230°F) or below. bonds exceptionally well through the various stamping lubricants typically present on metals, eliminating the need for advance cleaning and surface preparation. provides excellent resistance to moisture, sunlight, salt spray and thermal cycling; sustains short exposure to postbakes up to 204°C (400°F).

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.40 - 10.0 lb/galResin
 11.5 - 12.4 lb/galHardener
Viscosity Measure 130000 - 400000 cStagitated sample, cps, Hardener
 100000 - 450000 cStagitated sample, cps, Resin
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 20 - 30 %Cured; ASTM D 638
Impact Test >= 90.0 in-lbCured; GM 9751P
Peel Strength >= 30.0 pliASTM D 1876
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 400 °F
Flash Point >= 93.0 °CClosed Cup
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 25.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceGrey PasteHardener
 White PasteResin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9151 / 232539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.