MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 7881 Computer-Imprintable Polyester Label Material
Categories: Polymer; Adhesive

Material Notes: Features:
  • Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. The topcoat also provides improved ink anchorage for traditional forms of press printing.
  • #300 adhesive bonds well to a wide variety of substrates including metals, high surface energy (HSE) plastics and low surface energy (LSE) plastics. It is ideal for applications requiring high initial adhesion especially to LSE plastic surfaces.
  • 55# densified kraft liner assures consistent die cutting.
  • 3M™ Label Material 7881 is UL recognized (Files MH11410) and CSA accepted (File 99316). See the UL and CSA listings for details
Applications:
  • Barcode labels and rating plates.
  • Property identification and asset labeling.
  • Warning, instruction, and service labels for durable goods.
  • Nameplates for durable goods.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.800 milAdhesive
 2.30 milFacestock
 3.20 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 0.5625 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 0.625 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 1.0625 pliPolycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 1.5625 pliLD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 1.75 pliHD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 1.75 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 1.8125 pliHD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 1.875 pliPolycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 1.875 pliLD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.00 pliLD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.00 pliHD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.125 pliLD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.1875 pliHD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.25 pliLD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.25 pliPolycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.375 pliPolypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.375 pliPolypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.50 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 2.50 pliHD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.625 pliStainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.625 pliGlass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.625 pliLD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.625 pliPolypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 2.75 pliPolycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
 2.75 pliPolypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.75 pliGlass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.8125 pliHD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 2.875 pliStainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 2.875 pliPolycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 3.00 pliGlass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
 3.125 pliStainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 3.125 pliGlass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 3.3125 pliPolypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 3.3125 pliStainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 3.375 pliPolypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 3.4375 pliPolycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 3.50 pliStainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 3.50 pliPolypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 3.6875 pliPolycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 3.75 pliGlass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
 3.8125 pliPolycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 4.125 pliPolypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 4.1875 pliGlass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 4.1875 pliStainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 4.25 pliStainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
 4.375 pliStainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 4.375 pliGlass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
 4.4375 pliGlass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive Carrier55# Densified kraft
Adhesive Type#300 Acrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33376 / 168123

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.