MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Thallium, Tl
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.85 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 204.38331995
Atomic Number 81
Thermal Neutron Cross Section 3.4 barns/atom
X-ray Absorption Edge 0.1447 ÅK
 0.80787 ÅLI
 0.84355 ÅLII
 0.97968 ÅLIII
Electrode Potential -0.336 V
Electronegativity 1.8Pauling
Ionic Radius 0.950 ÅCrystal Ionic Radius for Valence +3
 1.47 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 2.5 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 2.0
Hardness, Vickers 2.0
Tensile Strength, Ultimate 7.50 MPa
Elongation at Break 40 %in 125 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000150 ohm-cm
Magnetic Susceptibility -2.40e-7cgs/g
Critical Magnetic Field Strength, Oersted 176 - 180
Critical Superconducting Temperature 2.36 - 2.40 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 20.9 J/g
Heat of Vaporization 1231 J/g
CTE, linear 28.0 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.136 J/g-°C
Thermal Conductivity 39.4 W/m-K
Melting Point 304 °C
Boiling Point 1473 °C
 
Component Elements PropertiesOriginal ValueComments
Thallium, Tl 100 %
 
Descriptive Properties
CAS Number7440-28-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thorium, Th
Titanium, Ti
Osmium, Os; Annealed
Rhenium, Re; Annealed
Thulium, Tm

AMETl00 / 116

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.