MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 1034 Steel  (discontinued **)
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: This AISI/SAE steel was discontinued as a standard in 1968. Water-hardening steels suitable for small parts of moderate strength. Used in levers, bolts, nuts, studs and similar parts which are headed, upset, or extruded. This steel deleted as a SAE-AISI standard in 1968.

Key Words: AFNOR XC 38, JIS S 38 C, carbon steels, UNS G10340, ASTM A29, ASTM A181, SAE J118, SAE J412, DIN 1.1181, AFNOR XC 32, AFNOR XC 35
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccTypical for steels.
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 200 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steels.
Poissons Ratio 0.29Typical For Steel
Shear Modulus 80.0 GPaTypical for steels.
Izod Impact 75.0 JAs rolled
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000174 ohm-cm
@Temperature 20.0 °C
annealed specimen
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.7 µm/m-°C
@Temperature 15.0 - 75.0 °C
Specific Heat Capacity 0.472 J/g-°CTypical steel
Thermal Conductivity 43.6 W/m-K
@Temperature 100 °C
Estimated
 50.7 W/m-K
@Temperature 0.000 °C
Estimated
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.32 - 0.38 %
Iron, Fe 98.73 - 99.18 %As remainder
Manganese, Mn 0.50 - 0.80 %
Phosphorus, P <= 0.040 %
Sulfur, S <= 0.050 %

References for this datasheet.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 425°C (800°F) temper, 25 mm (1 in.) round
AISI 1030 Steel, as rolled
AISI 1035 Steel, as rolled, 19-32 mm (0.75-1.25 in) round
AISI 4130 Steel, annealed at 865°C (1590°F)
AISI 5135 Steel

M1034A / 6912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.