MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.00 - 3.50 g/ccAverage value: 1.07 g/cc Grade Count:263
Water Absorption 0.100 - 3.50 %Average value: 0.477 % Grade Count:40
Moisture Absorption at Equilibrium 0.200 - 0.310 %Average value: 0.264 % Grade Count:23
Water Absorption at Saturation 0.100 - 1.60 %Average value: 0.997 % Grade Count:7
Maximum Moisture Content 0.0100 - 0.100Average value: 0.0253 Grade Count:17
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cmAverage value: 0.00518 cm/cm Grade Count:182
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cmAverage value: 0.00585 cm/cm Grade Count:13
Melt Flow 0.100 - 43.0 g/10 minAverage value: 10.1 g/10 min Grade Count:257
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102 - 103Average value: 103 Grade Count:3
Hardness, Rockwell R 78.0 - 118Average value: 103 Grade Count:157
Ball Indentation Hardness 74.0 - 105 MPaAverage value: 92.3 MPa Grade Count:17
Tensile Strength, Ultimate 24.0 - 138 MPaAverage value: 40.6 MPa Grade Count:107
Tensile Strength, Yield 22.1 - 93.1 MPaAverage value: 42.3 MPa Grade Count:197
Elongation at Break 3.00 - 87.0 %Average value: 24.3 % Grade Count:142
Elongation at Yield 2.00 - 12.0 %Average value: 3.49 % Grade Count:69
Modulus of Elasticity 1.40 - 5.33 GPaAverage value: 2.12 GPa Grade Count:93
Flexural Yield Strength 0.379 - 121 MPaAverage value: 66.5 MPa Grade Count:183
Flexural Modulus 0.210 - 13.1 GPaAverage value: 2.30 GPa Grade Count:228
Compressive Yield Strength 47.5 - 50.6 MPaAverage value: 49.4 MPa Grade Count:10
Bearing Yield Strength 20.3 - 359 MPaAverage value: 133 MPa Grade Count:10
Shear Strength 37.2 - 40.1 MPaAverage value: 38.3 MPa Grade Count:10
Izod Impact, Notched 0.220 - 5.88 J/cmAverage value: 3.00 J/cm Grade Count:175
 0.461 - 3.80 J/cm
@Temperature -30.0 - 0.000 °C
Average value: 1.75 J/cm Grade Count:16
 0.48051 - 3.00 J/cm
@Temperature -40.0 - 0.000 °C
Average value: 1.75 J/cm Grade Count:9
 0.48051 - 3.00 J/cm
@Thickness 3.17 - 3.20 mm
Average value: 1.75 J/cm Grade Count:9
Izod Impact, Unnotched 3.25 - 5.07 J/cmAverage value: 4.28 J/cm Grade Count:4
 0.588399 - 3.04006 J/cm
@Temperature -30.0 - -20.0 °C
Average value: 1.99 J/cm Grade Count:6
 0.588399 - 3.04006 J/cm
@Thickness 3.20 - 6.40 mm
Average value: 1.99 J/cm Grade Count:6
Izod Impact, Notched (ISO) 10.0 - 43.0 kJ/m²Average value: 24.2 kJ/m² Grade Count:71
 7.00 - 72.0 kJ/m²
@Temperature -40.0 - -20.0 °C
Average value: 13.9 kJ/m² Grade Count:30
 12.0 - 12.0 kJ/m²
@Temperature -40.0 - -40.0 °C
Average value: 13.9 kJ/m² Grade Count:1
 12.0 - 12.0 kJ/m²
@Thickness 4.00 - 4.00 mm
Average value: 13.9 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) 55.0 kJ/m² - NBAverage value: 81.1 kJ/m² Grade Count:17
 80.0 - 100 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 95.7 kJ/m² Grade Count:7
Charpy Impact Unnotched 8.00 J/cm² - NBAverage value: 14.1 J/cm² Grade Count:43
 7.00 J/cm² - NB
@Temperature -40.0 - -20.0 °C
Average value: 10.8 J/cm² Grade Count:37
Charpy Impact, Notched 0.800 - 6.30 J/cm²Average value: 2.68 J/cm² Grade Count:84
 0.600 - 2.20 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 1.26 J/cm² Grade Count:38
Gardner Impact 10.6 - 46.1 JAverage value: 24.0 J Grade Count:15
 4.00 - 24.7 J
@Temperature -29.0 - -29.0 °C
Average value: 17.8 J Grade Count:3
Instrumented Impact Total Energy 19.0 - 54.0 JAverage value: 37.0 J Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cmAverage value: 6.22e+15 ohm-cm Grade Count:38
Surface Resistance 1.00e+13 - 2.00e+16 ohmAverage value: 2.41e+15 ohm Grade Count:21
Dielectric Constant 2.70 - 3.10Average value: 2.96 Grade Count:19
Dielectric Strength 7.00 - 48.0 kV/mmAverage value: 27.1 kV/mm Grade Count:41
Dissipation Factor 0.00480 - 0.0900Average value: 0.0322 Grade Count:19
Arc Resistance 0.000 - 120 secAverage value: 80.0 sec Grade Count:6
Comparative Tracking Index 400 - 600 VAverage value: 594 V Grade Count:24
Hot Wire Ignition, HWI 7.00 - 120 secAverage value: 20.9 sec Grade Count:15
High Amp Arc Ignition, HAI 10.0 - 200 arcsAverage value: 142 arcs Grade Count:15
High Voltage Arc-Tracking Rate, HVTR 0.000 - 150 mm/minAverage value: 28.7 mm/min Grade Count:14
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.8 - 110 µm/m-°CAverage value: 86.2 µm/m-°C Grade Count:59
CTE, linear, Transverse to Flow 86.0 - 110 µm/m-°CAverage value: 96.2 µm/m-°C Grade Count:5
Thermal Conductivity 0.150 - 0.180 W/m-KAverage value: 0.169 W/m-K Grade Count:9
Maximum Service Temperature, Air 60.0 - 90.0 °CAverage value: 67.1 °C Grade Count:7
Hot Ball Pressure Test 90.0 - 95.0 °CAverage value: 93.1 °C Grade Count:13
Deflection Temperature at 0.46 MPa (66 psi) 63.0 - 121 °CAverage value: 94.3 °C Grade Count:111
Deflection Temperature at 1.8 MPa (264 psi) 58.0 - 220 °CAverage value: 88.6 °C Grade Count:221
Vicat Softening Point 88.0 - 128 °CAverage value: 100 °C Grade Count:178
Glass Transition Temp, Tg 105 - 108 °CAverage value: 107 °C Grade Count:4
UL RTI, Electrical 50.0 - 80.0 °CAverage value: 63.2 °C Grade Count:26
UL RTI, Mechanical with Impact 50.0 - 80.0 °CAverage value: 64.4 °C Grade Count:16
UL RTI, Mechanical without Impact 50.0 - 80.0 °CAverage value: 64.4 °C Grade Count:16
Flammability, UL94 HB - 5VAGrade Count:186
Flame Spread 28.0 - 55.0 mm/minAverage value: 42.7 mm/min Grade Count:3
Glow Wire Test 550 - 700 °CAverage value: 663 °C Grade Count:23
 
Optical PropertiesOriginal ValueComments
Haze 2.00 - 2.50 %Average value: 2.14 % Grade Count:5
Gloss 6.00 - 99.0 %Average value: 82.5 % Grade Count:18
Yellow Index 13.0 - 31.0 %Average value: 18.0 % Grade Count:4
Transmission, Visible 88.0 - 90.0 %Average value: 89.3 % Grade Count:5
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 270 °CAverage value: 230 °C Grade Count:28
Nozzle Temperature 180 - 275 °CAverage value: 228 °C Grade Count:25
Adapter Temperature 200 - 250 °CAverage value: 226 °C Grade Count:6
Die Temperature 113 - 250 °CAverage value: 205 °C Grade Count:6
Melt Temperature 170 - 302 °CAverage value: 223 °C Grade Count:111
Mold Temperature 20.0 - 100 °CAverage value: 59.1 °C Grade Count:119
Injection Velocity 40.0 - 240 mm/secAverage value: 216 mm/sec Grade Count:20
Roll Temperature 60.0 - 100 °CAverage value: 80.8 °C Grade Count:6
Drying Temperature 70.0 - 100 °CAverage value: 82.7 °C Grade Count:111
Moisture Content 0.0400 - 0.200 %Average value: 0.127 % Grade Count:13
Injection Pressure 2.76 - 150 MPaAverage value: 41.7 MPa Grade Count:43
Vent Depth 0.00254 - 0.0510 cmAverage value: 0.0172 cm Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade

O1103 / 77795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.