MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe LSS™ 440C Stainless Steel Knife (ASTM A276)
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel

Material Notes: TLS 440C Stainless Knife Steel is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 60 HRC. The high carbon content results in a hard matrix and numerous chromium carbides in the microstructure, which in turn provide excellent wear resistance and retention of cutting edges. TLS 440C stainless knife steel should be considered for applications such as specialty knives, industrial knives, scissors, surgical knives, and other applications which require a combination of corrosion resistance, wear resistance, or edge retention.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.62 g/cc
Density 0.275 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 57.5Oil Quenched from 1066°C, 30 minutes
 57.5Air Quenched from 1066°C, 30 minutes
 59Air Quenched from 1010°C, 30 minutes
 60Oil Quenched from 1010°C, 30 minutes
 61Air Quenched from 1038°C, 30 minutes
 62Oil Quenched from 1038°C, 30 minutes
Modulus of Elasticity 29000 ksi
Machinability 30 - 40 %1% Carbon Steel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000060 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µm/m-°C
@Temperature 20.0 - 200 °C
 11.2 µm/m-°C
@Temperature 20.0 - 600 °C
Specific Heat Capacity 0.110 BTU/lb-°F
Thermal Conductivity 24.2 W/m-K
@Temperature 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.05 %
Chromium, Cr 17 %
Iron, Fe 81.15 %
Manganese, Mn 0.40 %
Molybdenum, Mo 0.40 %
Silicon, Si 0.40 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
440C Martensitic Stainless Steel (UNS S44004)
AISI 440 Stainless Steel
Latrobe LSS™ S7 Shock-Resisting Tool Steel (ASTM S7)
Kinetics MIM 440C Stainless Steel
440C Modified Stainless Steel (Composition Spec)

NTIMK134 / 19481

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.