MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zircar Zirconia ZYK-15 Zirconia Cloth Insulation
Categories: Ceramic; Machinable Ceramic; Oxide; Zirconium Oxide

Material Notes: Zirconia Cloth Type ZYK-15 is a tricot knit cloth nominally 0.012” thick composed of yttria stabilized zirconia fibers. This material offers extreme temperature and chemical resistance in a flexible form and provides the lowest thermal conductivity of any commercially available refractory fiber material. ZYK-15 cloth is ideal for temperatures up to 2200°C. The melting temperature is 2590°C. It is suitable for applications such as high energy battery separators, thermal insulation in crystal growing furnaces, and for the filtration of hot gases.

ZYK-15 is a true textile constructed of essentially continuous individual filaments fabricated in a tricot knit form. It requires neither binders nor supporting wires in its construction and will comply somewhat to both tensile and compressive forces due to the mechanical interlocking of their fibers. Elongation of 4 to 8% before breaking allows ZYK-15 to conform to irregular surfaces. ZYK-15 can be compressed up to two-thirds of its normal thickness and still recover a major fraction of its original dimension with little fiber damage.

The fine capillary and pore structure of ZYK-15, in combination with the hydrophilic nature of zirconia and the serrated surface of the individual fibers in the knit threads, impart excellent wetting solution retention and wicking characteristics to this material.

Features:

  • Low Thermal Conductivity
  • High Purity
  • Extreme High Temperature Stability
  • Fibers Stabilized with ~10 wt% Yttria
  • Can be Cemented with Zircar Zirconia Cement Type ZR-CEM
  • Can be Rigidized with Zircar Zirconia Rigidizer Type ZR-RIG
  • Easily Cut to Size
  • Available ‘off the shelf’

Information provided by Zircar Zirconia.

Key Words: ZrO2, zirconium oxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.680 g/cc
Porosity 85 %Bulk
Thickness 12.0 mil
Vapor Pressure 8.00e-12 torr
@Temperature 1370 °C
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.130 BTU/lb-°F
@Temperature 93.3 °C
 0.180 BTU/lb-°F
@Temperature 2370 °C
Melting Point 2590 °C
Maximum Service Temperature, Air 2200 °CContinuous
Shrinkage 4.3 %
@Temperature 899 °C,
Time 3600 sec
1 hour isothermal soak at 1650°F
 
Component Elements PropertiesOriginal ValueComments
HfO2 1.0 - 2.0 %
Y2O3 10 %
ZrO2 88 - 89 %
 
Descriptive Properties
Tensile Strength per Unit Width166 gram/cm width
Trace Impurities<0.25%
Weight Per Area207 g/m2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled
CoorsTek Alumina-Zirconia Composite, AZ-25
Polyplastics Duracon® TD-15 Acetal Co-polymer (POM), High impact, Flexible
Dymax 930 Coil Terminating, Tamper proofing and Structural Electronic Bonder
Dymax 928 Coil Terminating, Tamper proofing and Structural Electronic Bonder

C6ZIR018 / 2774

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.