Base Polymer: Polycarbonate Filler/Additive System: special filler, UV stabilized Special Features: Translucent, light scattering, high light diffusion, good flow Market Segment: Automotive, Lighting Application Area: Lighting, light transparent components Typical Application: Lamp covers, display elements, operating elements Information provided by Albis Plastics |