MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Datum Alloys Nickel Plated Steel Strip and Tags
Categories: Metal; Ferrous Metal

Material Notes: Nickel plated steel is suited for links for battery connections, to link cells together either as a single tag from cell to cell or as a special etched or stamped tag, that can link multiple cells. This material is both easy to spot weld and solder. It can be used as a substitute for nickel depending on the battery pack requirement, and can be used as electronic parts.

Apart from standard coil and plain tags, this material is often used for H Tags, the industry known 1404 Tag, and PCB board battery tags. Typically, it has 2 microns of nickel plate on both sides.

Information provided by Datum Alloys.

Key Words: Battery Connectors
Vendors: Datum Alloys is the leader in precision alloys for niche applications such as advanced stainless steel foils for the Surface Mount Technology (SMT) industry and of nickel and nickel plated tags used in the manufacture of battery packs. Call +1 607 239 6274 or visit datumalloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 80 - 11080 - 110
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Iron, Fe 99.6 %99.6 %
Manganese, Mn 0.080 %0.080 %
Phosphorus, P 0.012 %0.012 %
Silicon, Si 0.020 %0.020 %
Sulfur, S 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® 328 Copper Alloy
CMW® 3 Copper Alloy
CMW® 28 Copper Alloy
Cadi 1815 Copper Alloy
AISI 1018 Steel, cold drawn

NDATUM91 / 198186

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.