MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, and processability.

Mylar® A films have balanced tensile properties and excellent resistance to moisture and most chemicals. They can withstand temperature extremes from -100°F to 300ºF. Mylar® does not become brittle with age under normal conditions, because it contains no plasticizers.

Typical Applications:

  • Apparel stays
  • Book jackets
  • Carbon ribbon
  • Control Tape
  • Drumheads
  • Duct Liners
  • Identifications
  • Membrane touch switches
  • Metallized Base
  • Pressure Sensitive Labels (plain or metallized)
  • Protective surfacing
  • Release liners
  • Roll leaf (hot stamping)
  • Spirit Masters
Approvals: FDA Food Contact Status - All gauges of Mylar® A comply with the Food and Drug Administration regulation 21 CFR 177.1630 -- Polyethylene phthalate polymers. This regulation describes films which may be safely used in contact with all types of food excluding alcoholic beverages. Uncoated films such as Mylar® A can be used to contain foods during oven cooking or oven baking at temperatures above 250 °F. UL 94 VTM-2 - for 92-1400 gauge (0.023 - 0.35mm). UL Recognition - for 92-500 gauge (0.023-0.13mm) HWI=5, HAI=4, CTI=1; for 700-1400 gauge (0.18-0.35mm) HWI=4, HAI=0, CTI=1

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ASTM D1505
Viscosity Measurement 0.560.56ASTM D2857
Thickness 254 microns10.0 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %ASTM D882A
Film Elongation at Break, TD 140 %140 %ASTM D882A
Tensile Modulus 3.50 GPa507 ksiASTM D822
Compressive Yield Strength  58.3 MPa
@Strain 2 %
8450 psi
@Strain 2 %
ASTM D695
 116 MPa
@Strain 1 %
16800 psi
@Strain 1 %
1% offset; ASTM D695
 207 MPa
@Strain 23 %
30000 psi
@Strain 23 %
at max stress; ASTM D695
Compressive Modulus 2.85 GPa413 ksiASTM D695
Poissons Ratio 0.380.38Typical Mylar® before yield
 0.580.58Typical Mylar® after yield
Shear Strength 134 MPa19500 psiPunch test on film, unusually high for a polymer; ASTM D732
Film Tensile Strength at Break, MD 186 MPa27000 psiASTM D882A
Film Tensile Strength at Break, TD 200 MPa29000 psiASTM D882A
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 - 600 V400 - 600 V
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 sec
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcs
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 30.0 - 50.0 °C
9.44 µin/in-°F
@Temperature 86.0 - 122 °F
92 Gauge; ASTM D696
Specific Heat Capacity 1.17 J/g-°C0.280 BTU/lb-°F
Thermal Conductivity 0.155 W/m-K
@Temperature 25.0 - 75.0 °C
1.07 BTU-in/hr-ft²-°F
@Temperature 77.0 - 167 °F
Melting Point 254 °C489 °FDSC
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Shrinkage, MD 1.5 %
@Temperature 150 °C,
Time 1800 sec
1.5 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 1.1 %
@Temperature 150 °C,
Time 1800 sec
1.1 %
@Temperature 302 °F,
Time 0.500 hour
Unrestrained
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.64 - 1.671.64 - 1.67typical of Mylar®
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Yield (nominal)2000 in2/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Teijin Films Mylar® A Polyester Film, 1400 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge
DuPont Teijin Films Mylar® A Polyester Film, 48 Gauge
DuPont Teijin Films Mylar® 50 OL Polyester Film, Ovenable Lidding, Heat Sealable, 50 Gauge
DuPont Teijin Films Mylar® 850H Polyester Film, 48 Gauge

PDTZ9282 / 139604

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.