MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) RHODOLINE® 4100 Surfactant
Categories: Fluid

Material Notes: Standard Applications: RHODOLINE® 4100 is a very effective APE free anionic wetting and dispersing agent in both water and solvent based industrial systems. RHODOLINE® 4100 exhibits improved film properties including gloss, color acceptance and adhesion. Recommended usage levels typically are 0.1 – 0.5% active as wetting agents for paint formulations, 1 – 2% active for pigment wetting and 5 – 20% active on the pigment weight for pigment dispersing.

Chemical Name: Anionic Wetting and Dispersing Agent

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH <= 1.510% aqueous solution
Viscosity 1050 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.80 %Karl Fischer; RPG16
 
Descriptive Properties
AppearanceClear to cloudy liquidRPG31
Content100%Active

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) RHODOLINE® 4160 Surfactant
Solvay RHODAFAC® RS-610/A25 Surfactant
Solvay RHODAFAC® RS-960 Surfactant
Solvay RHODAFAC® RS-710 Surfactant
Solvay RHODAFAC® RS-710 E Surfactant

PSOLVAY802 / 218530

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.