MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical TR300 MABS, Flame Retardant, Transparency  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Material Notes: Feature: Injection Molding, Flame Retardant, Transparency

Application: Electric/Electronic Applications (TV, Monitor Housing) IT/OA device

CAS No. 9010-94-0 and 25713-60-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Water Absorption 0.50 - 1.0 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 35 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength, Yield 430 kg(f)/cm²
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Break 30 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Elongation at Yield >= 5.0 %
@Thickness 3.20 mm
50 mm/min; ASTM D638
Tensile Modulus 21000 kg(f)/cm²
@Thickness 3.20 mm
1 mm/min; ASTM D638
Flexural Yield Strength 700 kg(f)/cm²
@Thickness 6.40 mm
15 mm/min; ASTM D790
Flexural Modulus 22000 kg(f)/cm²
@Thickness 6.40 mm
15 mm/min; ASTM D790
Izod Impact, Notched 10.0 kg-cm/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 11.0 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 4.00 kg-cm/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
ASTM D256
 4.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
@Thickness 6.40 mm
Unannealed; ASTM D648
Vicat Softening Point 90.0 °C
@Load 5.00 kg
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C
@Thickness >=1.50 mm
UL 746B
UL RTI, Mechanical with Impact 50.0 °C
@Thickness >=1.50 mm
UL 746B
UL RTI, Mechanical without Impact 50.0 °C
@Thickness >=1.50 mm
UL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chi Mei Polylac® PA-758 ABS - Transparent
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
Lotte Advanced Materials Starex® TX-0520T Transparent Grade ABS
Chi Mei Polylac® PA-758R ABS - Transparent

PLAY088 / 148096

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.