MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell ArmaFORM® FR100 PET foam core
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: With ArmaFORM® PET FR we offer a Polyethylene Therephthalate (PET) based structural foam core which has been designed for the more stringent flame, smoke and toxicity requirements (FST) in the railway industry.

Key characteristics of ArmaFORM® PET foam cores in railway applications:

  • improved energy efficiency in operation
  • increased freight and passenger revenues
  • reduced operational costs over its life span
  • reduced installation costs and time
  • superior FST properties
  • excellent insulation properties for efficient heating/cooling systems
  • less CO2 emissions in operation
  • less energy/fuel consumption in operation
  • full recyclability at the end of the train's life cycle

Information provided by Armacell®

Key Words: Green; recyclable
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.20 lb/ft³ISO 845
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 350 psiASTM C297
Elongation at Yield 15 %Shear Strain; ISO 1922
Tensile Modulus 15225 psiASTM C297
Compressive Strength 220 psiISO 844
Compressive Modulus 10150 psiISO 844
Shear Modulus 2.90 ksiISO 1922
Shear Strength 125 psiISO 1922
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.236 BTU-in/hr-ft²-°F
 
Descriptive Properties
Fire PerformanceRailway Vehicles Construction; FlammabilityM1; NF F16-101
 Railway Vehicles Construction; Smoke DensityF1; NF F16-101
 Railway Vehicles; DrippingST2; DIN 5510-2
 Railway Vehicles; Edge ignitionK1; DIN 5510-2
 Railway Vehicles; FlammabilityS4; DIN 5510-2
 Railway Vehicles; FSTconform; CEN/TS 45545-2
 Railway Vehicles; Smoke DensitySR2; DIN 5510-2
 Railway Vehicles; Toxicity<.01; DIN 5510-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik Kanthal R63C Resistance Heating Wire and Strip
Armacell FR100 PET Foam
Armacell ArmaFORM® GR70 PET foam core
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged

PARMC10 / 183702

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.