MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silver Iodide, AgI, (Miersite)
Categories: Ceramic; Halide; Other Engineering Material; Semiconductor

Key Words: Halide; Semiconductor
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.67 g/cc
Solubility in Water 0.0000030 %
a Lattice Constant 6.502 Å
Molecular Weight 234.772 g/mol
Volume Compressibility, 10^-10 m²/N 0.41
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 2.5
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 10
Band Gap 2.22 eV
Electron Mobility, cm²/V-s 30
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 40.0 J/gCrystal structure not specified.
CTE, linear -2.50 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.232 J/g-°C
Thermal Conductivity 0.420 W/m-K
Melting Point 558 °C
Boiling Point 1506 °C
Heat of Formation 389 kJ/mol
Debye Temperature -139 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 2.22
 
Descriptive Properties
CAS Number7783-96-2
Crystal StructureCubicSphalerite Structure - Space Group F(-4)3m

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver Iodide, AgI, (Iodargirite)
Tin Selenide, SnSe
Silver Indium Selenide, AgInSe2
Tin Telluride, SnTe
MV Labs AG600 AgI Silver iodide

DSEN53 / 3065

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.