MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives Thermoset™ SC-300M Silicone Gel Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Encapsulation Grade

Material Notes: SC-300M is a two-part, rapid curing, platinum-catalyzed, addition cured, silicone gel. It has an extremely soft, gel-like consistency when cured, and has excellent unprimed adhesion to most substrates. SC-300M provides thermal, mechanical, and vibration dampening, and has excellent electrical properties.

SC-300M does not generate an exotherm during cure and it is resistant to reversion. It exhibits very low shrinkage and the cure may be accelerated by the application of heat. SC-300M has excellent heat stability and relatively low toxicity.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 g/cc0.990 g/ccSTM 2
Volatiles 0.010 %0.010 %
Viscosity 200 cP200 cPSTM 1
 
Mechanical PropertiesMetricEnglishComments
Penetration 5.0
@Load 0.0195 kg
5.0
@Load 0.0430 lb
mm
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.90e+14 ohm-cm
@Temperature 25.0 °C
9.90e+14 ohm-cm
@Temperature 77.0 °F
ASTM D257
Dielectric Constant 2.7
@Frequency 100000 Hz,
Temperature 25.0 °C
2.7
@Frequency 100000 Hz,
Temperature 77.0 °F
ASTM D150
Dissipation Factor 0.0050
@Frequency 100000 Hz,
Temperature 25.0 °C
0.0050
@Frequency 100000 Hz,
Temperature 77.0 °F
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 326 µm/m-°C
@Temperature 25.0 °C
181 µin/in-°F
@Temperature 77.0 °F
Thermal Conductivity 0.154 W/m-K1.07 BTU-in/hr-ft²-°FASTM D2214
Maximum Service Temperature, Air 200 °C392 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min
@Temperature 25.0 °C
30 min
@Temperature 77.0 °F
Gel Time 50.0 min
@Temperature 25.0 °C
50.0 min
@Temperature 77.0 °F
Shelf Life 6.00 Month
@Temperature 25.0 °C
6.00 Month
@Temperature 77.0 °F
 
Descriptive Properties
Mix Ratio1:1by weight, by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
300M Ultrahigh Strength Steel
CHT Group QGel 319 Optically Clear Silicone Gel
Lord Adhesives Thermoset™ SC-102 Unfilled Silicone Encapsulant
Master Bond MasterSil 415 One Component Room Temperature Curing, Transparent Silicon
Assab Steels 705M Machinery Steel

PLORD064 / 86072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.