MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary Evoprene™ 029 Standard SBS Thermoplastic Elastomer Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.
Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat hanger pads, toy components

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccISO 2782
Viscosity Measurement 11
@Temperature 150 °C
Kg/cm2; Macklow-Smith extrusion rheometer
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 92ISO 868
Hardness, Shore D 43
Tensile Strength 11.1 MPaISO 37
Elongation at Break 470 %ISO 37
100% Modulus 0.00770 GPa
@Strain 100 %
ISO 37
Tear Strength 61.0 kN/mISO 34-B
Compression Set 65 %
@Temperature 22.0 °C,
Time 259000 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 55.0 - 60.0 °C
Minimum Service Temperature, Air -60.0 °C
 
Descriptive Properties
Bonds withPolypropylene
Chemical ResistanceAcetoneModerate
 Acids up to 80%Moderate
 AlcoholGood
 AlkalisGood
 Brake fluidModerate
 Chlorinate solventsPoor
 DieselPoor
 Ethylene glycolExcellent
 GasolinePoor
 Salt solutionGood
 Soda lyeModerate
 Water, 23°CGood
 Water, 95°CPoor
Ozone ResistancePass - No Crack100 pphm / 200 hrs / 20% strain
TransparencyOpaque

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Evoprene™ HP 3712 High Performance Thermoplastic Elastomer
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ G 614 SEBS Thermoplastic Elastomer
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound

PGARY9620 / 140413

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.