MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NAECO® ELKONIUM® 34 platinum based alloy
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy

Material Notes: Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (1769(C) and good resistance to forming arcs. Low electrical conductivity (15% IACS) limits its application to low currents, usually below 5 amperes. Because of the high cost of the platinum ELKONIUM alloys, they are almost always supplied as composite contacts with thin facings of the ELKONIUM metal (silver brazed to nickel plated steel backings in the form of rivets, screws and weld buttons).

ELKONIUM 34, ELKONIUM 305 and ELKONIUM 306 alloys have lower ruthenium contents and are softer and more ductile. They can be headed into rivets over a limited range. All five alloys have low transfer characteristics and are used in voltage regulators and motor speed governors. They can be used as a positive contact paired with tungsten negative contact for improved transfer resistance. They also have high tarnish resistance and are suitable for many sensitive, low voltage applications.

Information provided by NAECO, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 20.3 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 15T 86annealed
 91cold worked
Tensile Strength, Ultimate 70000 psiannealed
 130000 psicold worked
Elongation at Break 5.0 %cold worked
 15 %annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000430 ohm-cm4 % IACS
 
Component Elements PropertiesOriginal ValueComments
Platinum, Pt 92 %
Ruthenium, Ru 8.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pt-3.5% Rh Alloy, Annealed
NAECO® ELKONIUM® 301 platinum based alloy
NAECO® ELKONIUM® 305 platinum based alloy
NAECO® ELKONIUM® 32 platinum based alloy
NAECO® ELKONIUM® 33 platinum based alloy

NCMV901 / 192385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.