MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
MetalTek MTEK 304L Cast UNS J92500 Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; Cast Stainless Steel; T 300 Series Stainless Steel

Material Notes: "300" series, general corrosion resistant alloy

Applications: Nuclear, chemical and food processing. Valve and pump trim.

Information provided by MetalTek

Key Words: Cast UNS J92500; Cast Grade CF3; Cast ASTM A351, A743, A744; AMS 5371 (Sand Casting); Wrought UNS S30403; Wrought Grade 304L
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 153
Tensile Strength, Ultimate >= 485 MPa
Tensile Strength, Yield >= 205 MPa
Elongation at Break >= 35 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.030 %
Chromium, Cr 17 - 21 %
Iron, Fe 63.47 - 75 %As Balance
Manganese, Mn <= 1.5 %
Nickel, Ni 8.0 - 12 %
Silicon, Si <= 2.0 %
 
Descriptive Properties
Heat TreatmentSol. Anneal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
310 Stainless Steel, annealed sheet
ASTM A204 Low Alloy Steel, Grade B
AISI Type 304L Stainless Steel
MetalTek MTEK 310 Cast UNS J94202 Austenitic Stainless Steel
MetalTek MTEK 347 Cast UNS J92710 Austenitic Stainless Steel

NMETEK043 / 18293

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.