MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Spartech DP5120 Talc Filled Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Talc Filler

Material Notes: Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food containers, and profile extruded and blown molded structural parts.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
@Temperature 22.8 °C
ASTM D792
Filler Content 20 %
Linear Mold Shrinkage 0.014 in/in0.125inch wall
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5100 psiASTM D638
Elongation at Break 30 %ASTM D638
Elongation at Yield 4.0 %ASTM D638
Flexural Modulus 280000 psisecant; ASTM D790
 380000 psitangent; ASTM D790
Izod Impact, Notched 0.900 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact >= 1.00 ft-lb
@Temperature -5.56 °C
ASTM D5420
 1.50 ft-lb
@Temperature 22.8 °C
ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 250 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °FASTM D648
 
Optical PropertiesOriginal ValueComments
Gloss 47 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
PolyMirae Moplen EP649N Polypropylene Copolymer
Total PPH 3429 Polypropylene, Injection Molding Grade
A. Schulman TPP20AE55BK 20% Talc-Filled, Heat-Stabilized, Homopolymer Polypropylene
Asahi Kasei Thermylene® P-20TC-0736 20% Talc Filled, Heat Stabilized Polypropylene

PSPAR125 / 78747

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.