MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kraton® G1650 E (SEBS) Linear Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms identified:
Kraton G1650 EU - supplied as undusted fluffy crumb
Kraton G1650 ES - supplied as fluffy crumb dusted with amorphous silica

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton G1650 E is used for formulating adhesives and coatings, as a base material for compound formulations, as a modifier of thermoplastics and as a modifier of bitumen. The inherent stability of the midblock suggests the use of G1650 E in applications that must withstand weathering and high processing temperatures.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Medical; Packaging and Polymod; Personal Care; Bitumen Modification; and Roads and Roofing

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccISO 2781
Volatiles <= 0.50 %KM 04
Brookfield Viscosity 1000 - 1900 cP
@Temperature 25.0 °C
20% Toluene solution; KM 06
Ash 0.40 - 0.60 %ES; ISO 247
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 34.47 MPaMeasured on films cast from a solution in toluene; ASTM D412
Elongation at Break 500 %Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 0.00560 GPa
@Strain 300 %
film cast from poluene solution; ASTM D412
 
Descriptive Properties
ContentAntioxidant>0.03%, KM 08
 Polystyrene27.7-30.7%, KM 03
 Total Extractables<1.0%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® G1652 E (SEBS) Linear Block Copolymer
Kraton® FG1924 G (SEBS) Linear Block Copolymer
Kraton® G1657 M (SEBS) Linear Block Copolymer
Kraton® G1654 E (SEBS) Linear Block Copolymer
Kraton® G1765X (EP)n Multi-Arm Copolymer

PKRA0230 / 49083

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.