MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Abatron AboSeal 8104-17 Acrylic-Latex Based Sealant and Caulk; High-Density
Categories: Polymer; Adhesive; Thermoset

Material Notes: AboSeal 8104-17 is 80% solids and acrylic-latex based. It comes as one package and in most colors. It is known for its high density. It is the same as 8104-16 for low-odor, adhesion, quick drying and paintability, stability, retention of properties as no sag, but it is not as heavy-duty. It is also slightly lower in price. It's as easy to use as 8104-16 and 8104-18.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 13.1 lb/gal
Solids Content 80 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 36
Tensile Strength at Break 7.00 psi
Elongation at Break 970 %
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 54.0 g/minSemco
 
Descriptive Properties
ColorMost Colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboSeal 8104-8 Polysulfide, Thixotropic Sealant and Caulk
Abatron AboSeal 8104-18 Vinyl-Acrylic-Latex Based Sealant and Caulk
Abatron AboSeal 8104-16 Acrylic-Latex Based Sealant and Caulk
Abatron AboSeal 8104-15 Polysulfide, Thixotropic or Self-Leveling Sealant and Caulk
Abatron AboSeal 8104-14 Polysulfide, Thixotropic Sealant and Caulk

PABC925 / 107909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.